主要工艺参数对生物油酚醛树脂胶合板甲醛和TVOC含量的影响

Translated title of the contribution: Effect of process parameters on formaldehyde and TVOC content in plywood bonded with bio-oil phenol formaldehyde resins

Ping Huang, Fan Yang, Liangliang Jia, Jian Li, Dongbing Li

Research output: Journal PublicationArticlepeer-review

Abstract

为探究制胶阶段和压板阶段的6个因素(生物油替代率、醛酚比、热压温度、热压时间、热压压力、涂胶量)对胶合板中甲醛和总挥发性有机物(TVOC)含量的影响,在单因素试验基础上,设计L25(56)正交试验对工艺参数进行优化.采用顶空固相微萃取法(HS-SPME)和气相色谱/质谱(GC/MS)联用技术对生物油酚醛树脂胶合板(BPFP)中游离甲醛和除甲醛外的TVOC、苯酚进行检测.结果表明:当生物油替代率为60%,醛酚比值(nF/nP)1.6,热压温度190℃,热压时间4 min,热压压力1.2 MPa,涂胶量为200 g/cm2时,胶合板中含甲醛最低.热压温度和压力对甲醛含量有显著的影响,生物油替代率和涂胶量对胶合板中游离甲醛含量的影响较小;在生物油替代率为60%,醛酚比值2.2,热压温度190℃,热压时间5.5 min,热压压力1.4 MPa,涂胶量为210 g/cm2时,胶合板中TVOC含量最低.
Translated title of the contributionEffect of process parameters on formaldehyde and TVOC content in plywood bonded with bio-oil phenol formaldehyde resins
Original languageChinese (Simplified)
Pages (from-to)38-44
Number of pages7
JournalBiomass Chemical Engineering
Volume55
Issue number2
DOIs
Publication statusPublished - 7 Apr 2021