Abstract
Geldart Group A powders are utilized in various industrial processes because of their good fluidization quality, which is closely related to fine content (≤ 45 μm). This work systematically investigated the effect of fine powders (≤ 20 μm) as additives on the fluidization quality of Group A powders. Three types of additives, Coal-15, GB-6, and SiO2-5 were added into the base powder FCC-76 (Group A) in various volume fractions. Among them, the addition of SiO2-5 showed a significant improvement on the fluidization quality of Group A powder, exhibiting lower minimum fluidization velocity and higher bed expansion, while the addition of Coal-15 slightly improved the fluidization quality. The addition of a high-volume fraction of GB-6 would turn Group A into Group C/A, exhibiting some fluidization characteristics of Group C particles. Overall, the fluidization advancement of Group A powders modulated by Group C additives has advantages for industrial processes, especially for gas-phase catalytic reactions.
Original language | English |
---|---|
Pages (from-to) | 684-692 |
Number of pages | 9 |
Journal | Powder Technology |
Volume | 377 |
DOIs | |
Publication status | Published - 2 Jan 2021 |
Externally published | Yes |
Keywords
- Bed expansion
- Fine content
- Fluidization quality
- Gas-solid fluidization
- Geldart group A powder
- Group C powder
ASJC Scopus subject areas
- General Chemical Engineering