Abstract
This study presents a way of using South African coal fly ash by extracting metals such as Al and Fe with concentrated sulphuric acid, and then using the solid residue as a feedstock for the synthesis of ZSM-5 zeolite. The percentage of aluminium and iron oxides decreased from 28.0 ± 0.2% and 5.0 ± 0.1% in coal fly ash to 24.6 ± 0.1% and 1.6 ± 0.01% in the acid treated coal fly ash respectively. The fly ash-based zeolite ZSM-5 sample synthesised from the solid residue after extraction of Al and Fe, contained 62% of ZSM-5 zeolite pure phase with a number of Brønsted acid site density of 0.61 mmol per gzeolite. By properly treating the as-prepared coal fly ash-based ZSM-5 zeolite, an active and selective methanol-to-olefins acid catalyst could be designed, leading to full methanol conversion during 15 h on stream. The optimised catalyst exhibited a cumulative methanol conversion capacity of 71 g(MeOHconverted)/g(catalyst) and a light olefin productivity of 21 g(C2=–C4=)/g(catalyst).
Original language | English |
---|---|
Pages (from-to) | 78-86 |
Number of pages | 9 |
Journal | Comptes Rendus Chimie |
Volume | 20 |
Issue number | 1 |
DOIs | |
Publication status | Published - 1 Jan 2017 |
Externally published | Yes |
Keywords
- Acid leaching
- Fly ash
- MTO catalyst
- Metal extraction
- ZSM-5 zeolite
ASJC Scopus subject areas
- General Chemistry
- General Chemical Engineering